On-line and post-mortem wear measurement of static counterpart in a ball-on-disk test

Authors

  • Y. Perez Delgado
  • K. Bonny
  • P. De Baets
  • V. Rodriguez
  • P. Neis
  • J. Sukumaran
  • O. Malek
  • J. Vleugels
  • B. Lauwers

DOI:

https://doi.org/10.21825/scad.v3i2.20569

Abstract

this paper presents an experimental evaluation of friction coefficient and wear of WC binderlessceramics. The tests were conducted at room temperature and atmospheric conditions according to theASTM G99-95a standard. Silicon carbide (SiC) balls were used as static counterpart. The tests wereperformed at a rotating sliding speed of 0.3 m/s and an initial mean Hertzian contact pressure of 1.9 GPa.The disk specimens were surface finished by grinding. On-line monitoring and post-mortem analysis withtwo independent techniques, i.e., surface profilometry and optical microscopy, were used to elucidate thetribological characteristics of the studied material. Results of the post-mortem measurements werecompared to a geometrical wear model for calculation of the volume of the worn cap of the ball. Thiscalculation appeared to be in good agreement with the on-line wear monitoring. The first 100 m of slidingwas identified as running-in period. Beyond a sliding distance of 100 m a steady stage in penetration depthwas reached, while a higher fluctuation in friction coefficient was observed, which could be attributed to theinteraction with wear particles and simultaneous formation and delamination of debris layer, polishing andabrasion.

Downloads

Published

2012-11-05

Issue

Section

Articles